Every floor system is only as good as the profile under it and the joints through it. This is the work that never shows in a brochure and causes most of the failures.
- Mechanical prep$0.50–$2.50/sf
- Polyurea joint fill$1.50–$3.50/LF
- Spall rebuild$15–$45+/LF
- ProfilesCSP 2–5
ICRI 310.2R concrete surface profiles
ICRI Guideline 310.2R defines ten concrete surface profiles (CSP 1–10), verified on site against rubber replica chips under raking light. Resinous floors live in CSP 2–5. Too smooth and the coating has nothing to grip; too rough and a thin coating telegraphs the profile and leaves peaks exposed.
| Profile | Texture | Method | Receives |
|---|---|---|---|
| CSP 2 | Light (0.1–0.25mm) | Diamond grinding | Thin-film sealers and coatings under 10 mils |
| CSP 3 | Medium-light | Light shot blast or coarse diamond grind | High-build epoxy 10–40 mils, MVB primers, ESD |
| CSP 4 | Medium | Medium shot blast | Heavy coatings and overlays 40–100 mils, MMA |
| CSP 5 | Medium-heavy | Heavy shot blast, or scarify + shot blast pass | Self-levelers, 1/4–3/8 in. urethane cement |
Grinding vs. shot blasting vs. scarifying
| Method | Profiles | Strengths | Watch for |
|---|---|---|---|
| Diamond grinding | CSP 1–3 | Dust-controlled with HEPA vacuums; removes thin coatings; flattens; edges and small rooms | Can polish over a surface instead of opening it; slower on large areas |
| Shot blasting | CSP 3–6 | Fast on open floors (thousands of sf per shift); clean, open profile; self-contained dust collection | Leaves "striping" if passes overlap poorly; cannot reach edges |
| Scarifying (milling) | CSP 4–9 | Removes thick coatings, mastic build-up and high spots fast | Micro-cracking: bruises the top layer — always follow with a shot-blast pass before coating |
| Mechanical prep scope | Rate |
|---|---|
| Large scale (10,000+ sf) | $0.50–$0.90/sf |
| Medium (2,000–10,000 sf) | $0.90–$1.50/sf |
| Small (under 2,000 sf) | $1.50–$2.50+/sf |
| Add: existing coating, glue, mastic or oil-contaminated slab | +$1.00–$3.00+/sf |
Prep is included in the system rates elsewhere on this site; it is broken out here and in the moisture calculator for scoping and for prep-only work. How these ranges are built.
Control joints under forklift traffic (ACI 302.1R)
Saw-cut control joints in a slab-on-grade are the weak line of every warehouse floor. Hard polyurethane forklift wheels hit unfilled joint edges thousands of times a day; the arris chips, the chip becomes a spall, the spall becomes a pothole that shakes loads and wrecks wheels and bearings. ACI 302.1R recommends filling joints in traffic areas with a semi-rigid filler that supports the edges.
| Work | Spec | Installed $/LF |
|---|---|---|
| Preventative joint filling | Clean to full depth, fill with semi-rigid polyurea (Shore A-85 to D-50), shave flush | $1.50–$3.50 |
| Remedial spalled joint rebuild | Saw-cut shoulders, chip out, prime, rebuild with rapid-set polyurea or epoxy mortar, re-saw and fill | $15.00–$45.00+ |
Early fill and separation: the shrinkage reality
Concrete keeps shrinking for months to years after the pour, and joints open as it does. Filling too early means the semi-rigid filler separates from one joint face or splits down the middle. The practical approach:
- Fill as late as the schedule allows — ideally 60–90 days or more after the pour, with the building conditioned
- Specify a re-fill/top-off visit for separations once the slab has stabilized; it is maintenance, not failure
- Never use a soft elastomeric sealant in traffic joints — it does not support the edges
- Rebuild spalls before polishing or coating; a coating will not hold a broken arris
Get the slab walked before the budget is locked